I. Key boiler water quality control indicators
Boiler feed water quality control mainly focuses on the following key chemical indicators to prevent scale formation, reduce corrosion, and ensure steam purity.
- Hardness: Hardness is an indicator of the calcium and magnesium ion content in water and is the main cause of scale formation on boiler heating surfaces. Scale has extremely low thermal conductivity, leading to increased fuel consumption and excessively high metal wall temperatures. According to the latest testing standards, hardness measurement is generally based on Ca²⁺ and Mg²⁺ as the basic units.
- pH value: The pH value controls the corrosiveness of the water system. Boiler water usually needs to maintain an alkaline environment to form a protective film and prevent acidic corrosion of metals. For low-pressure boilers, boiler water is generally required to be maintained in an alkaline range; for high-pressure boilers, more precise control is required to prevent caustic embrittlement.
- Dissolved oxygen: Dissolved oxygen is one of the main factors causing corrosion of the boiler feed water system and boiler drum metals. It must be removed through thermal deaeration or chemical deaeration (such as adding sodium sulfite or hydrazine) to prevent pitting corrosion.
- Salt content and alkalinity: Excessively high salt content can cause foaming in the boiler water, resulting in priming and carryover and contaminating steam quality. Excessively high alkalinity may cause caustic embrittlement (intergranular corrosion) of metal components, especially for boilers with rolled joint structures, where the relative alkalinity must be strictly controlled.
To meet the above water quality requirements, a series of treatments must be applied to the raw water.
- Pretreatment: For water sources with high suspended solids content such as surface water, flocculation, sedimentation, and filtration are needed to remove suspended solids and organic matter. This step purifies the water quality, creating conditions for subsequent deep treatment.
- Softening and demineralization: Softening mainly uses ion exchange resin to remove calcium and magnesium ions from the water through sodium ion exchange, preventing scale on heating surfaces. This is the most common treatment method for industrial boilers. Demineralization: for high-pressure and above boilers, reverse osmosis (RO), electrodialysis (ED), or ion exchange demineralization systems are needed to thoroughly remove various salts (cations and anions) from the water and produce high-purity demineralized water.
- Deaeration: Thermal deaeration is the most common method, heating the feed water to boiling temperature to release dissolved oxygen. In addition, for hot water boilers, vacuum deaeration or chemical deaeration (such as adding sodium sulfite) can be used, and the sulfite content in the boiler water should be monitored.
- Internal chemical treatment: Even after external treatment, chemicals such as phosphate must be added to the boiler water to convert residual hardness into mobile sludge, which is discharged through blowdown to prevent secondary scale formation.
Water quality monitoring and blowdown management
- Water quality management is a dynamic process; blowdown operations must be guided by regular monitoring.
- Sampling requirements: To ensure the accuracy of monitoring data, representative sampling points should be installed in the steam-water system, equipped with sampling coolers. The sample temperature should preferably be below 30°C to ensure the sample is representative and uncontaminated.
- Blowdown control: Blowdown controls the salt content of the boiler water and removes deposited sludge.
For boilers using softened water as make-up, the normal blowdown rate should not exceed 10%.
For boilers using demineralized water as make-up, the blowdown rate should not exceed 2%. It is also recommended to recover heat from continuous blowdown water to improve energy utilization.